Effects of homogeneous and inhomogeneous heating on rotating shrink fits with annular inclusion and functionally graded hub / Tunç Apatay,Eray Arslan and Werner Mack.

By: Apatay, TunçContributor(s): Arslanb, Eray | Mackb, WernerCall Number: Repr.M47 Material type: ArticleArticleSubject(s): Functionally graded material | Hollow cylinders | Interference fit | Rotation | Temperature cycle In: Journal of Thermal Stresses 42 (11)2019:1458-1479Summary: For given geometrical properties of a shrink fit, the interface pressure is decisive for reliable operation and should stay as large as possible during operation. Using an appropriate functionally graded material for the hub facilitates a less decreasing interface pressure with increasing angular speed and, moreover, substantial weight-reduction. However, temperature cycles may influence the interface pressure considerably, and if partial plastification occurs, even a permanent decrease may result. These issues are discussed by analytical means, and both homogeneous and inhomogeneous temperature fields in an initially elastic shrink fit with hollow steel inclusion and steel-aluminum FGM-hub are considered.
No physical items for this record

สนใจติดต่อขอรับบริการเอกสารฉบับเต็มที่ one stop service (สำนักหอสมุดฯ) หรือ e-mail ([email protected]) โทร. 0 2201 7254-56, 0 2201 7287-89 (จัดเก็บชั้น 5 - Repr.M47)

YJ2019 M11

For given geometrical properties of a shrink fit, the interface pressure is decisive for reliable operation and should stay as large as possible during operation. Using an appropriate functionally graded material for the hub facilitates a less decreasing interface pressure with increasing angular speed and, moreover, substantial weight-reduction. However, temperature cycles may influence the interface pressure considerably, and if partial plastification occurs, even a permanent decrease may result. These issues are discussed by analytical means, and both homogeneous and inhomogeneous temperature fields in an initially elastic shrink fit with hollow steel inclusion and steel-aluminum FGM-hub are considered.

There are no comments on this title.

to post a comment.